Chinese character name Grade alloy element use Amount added Operating temperature °C performance
Aluminum Copper ALC u50 Cu48~52 Adjust alloy composition depending on demand 570~600 crisp
Aluminum silicon ALSi20 Si18~20 Adjust alloy composition depending on demand 700~800 crisp
Aluminum manganese ALMn10 Mn9~11 Adjust alloy composition depending on demand 770~830 tough
Aluminum manganese ALMn20 Mn18~22 Adjust alloy composition depending on demand 780~850 tough
Aluminum Titanium ALTi5 Ti4~6 Grain refinement, improve plasticity depending on demand 1020~1070 Easy to segregate
Aluminum Titanium ALTi10 Ti9~11 Grain refinement, improve plasticity depending on demand 1020~1070 Easy to segregate
Aluminum Nickel ALTi10 Ni9~11 Improve plasticity depending on demand 680~730 tough
aluminum chrome ALCr5 Cr4~6 Improve plasticity and improve performance depending on demand 900~1000 Easy to segregate
aluminum chrome ALCr10 Cr9~11 Improve plasticity and improve performance depending on demand 900~1000 Easy to segregate
aluminum chrome ALCr20 Cr18~22 Improve plasticity and improve performance depending on demand 910~1020 Easy to segregate
Aluminum zirconium ALZr5 Zr4~6 Improve plasticity and improve performance depending on demand 800~850 Easy to segregate
Aluminum Antimony ALSb4 Sb3~5 Improve plasticity and improve performance depending on demand 660 Easy to segregate
Aluminum Antimony ALSb10 Sb9~11 Improve plasticity and improve performance depending on demand 660 Easy to segregate
Aluminum iron ALFe20 Fe18~22 Improve plasticity and improve performance depending on demand 1020 crisp
Aluminum beryllium ALBe1 Be0.9~1.2 Improve plasticity and improve performance depending on demand 820 tough
Aluminum beryllium ALBe3 Be2~4 Improve plasticity and improve performance depending on demand 820 tough
Aluminum beryllium ALBe5 Be4.5~5.5 improves plasticity and performance depending on demand 820 tough
Aluminum Boron ALB3 B2.5~3.5 Reduce resistivity, improve conductivity, grain refinement 2~4% 800 tough
AlTiB (block/wire) ALTi5B1 Ti4.5~ 6 B0.9~1.2 Grain Refinement 0.5~2‰ 800 Easy to segregate
Aluminum lanthanum cerium ALRe10 Re9~11 Grain Refinement 2~3‰ 680 Easy to segregate
Aluminum titanium boron lanthanum cerium ALTi5B1Re10 Ti5B1Re10 Grain Refinement 1~3‰ 800 Easy to segregate
AlTiC ALTi5C0.2 Ti5C0.2 Grain Refinement 1~2‰ 1020~1070 Easy to segregate
Aluminum strontium ALSr10 Sr9~11 For long-term deterioration of aluminum-silicon alloys below silicon 13 1~2‰ 680~740 Easy to segregate
Aluminum yttrium ALY5 Y4~6 Improve plasticity and improve performance 1~2‰ 740~800 Easy to segregate
Aluminum bismuth ALBi10 Bi9~11 Improve plasticity and increase fluidity 1~2‰ 700~710 Easy to segregate
Aluminum scandium ALSc2 sc Adjust alloy composition and improve alloy properties depending on demand 700-800 tough
Aluminum cobalt ALCo5 co Adjust alloy composition and improve alloy properties depending on demand 720-750 tough
Aluminum molybdenum ALMo5-10 Mo Adjust alloy composition and improve alloy properties depending on demand 720-750 tough
Aluminum niobium ALNb10 Nb Increase fluidity and improve alloy properties depending on demand 690-750 tough
Aluminum cerium ALCe10 Ce Adjust alloy composition and improve alloy properties depending on demand 690-750 Easy to segregate
Aluminum tellurium ALTe5 Te Adjust alloy composition and improve alloy properties depending on demand 710-740 crisp
The chemical composition and impurities of aluminum master alloy ingots are produced according to the YS/T282-2000 standard, and other grades of master alloys and casting alloys can be produced according to user needs.